Differential Scanning Calorimeter
Advanced Differential Scanning Calorimeter with smart automation, wide temperature range, and precise heat measurement for reliable thermal analysis in research and production.
- Temperature range from -170°C to 600°C
- Automated measurement, evaluation, and LabV® data management
- Ideal for polymers, metals, and composites testing
Differential Scanning Calorimeter, Easy-to-use, robust, precise, optimized for everyday use – these are the features of the innovative DSC 300 Caliris®Classic. The unique design of this instrument encompasses everything needed for successful DSC investigations – regardless of whether the user is a beginner or an experienced professional The innovative software includes Auto Evaluation and Identify now meet the next generation of data management LabV®, which keeps track of the collected data and organizes it for a smooth laboratory workflow.
Features
- a compact design for more space in your lab
- touch display with LED status bar provides up-to-the-minute measurement information without the need to access your PC
- smart software that allows you to get started quickly with DSC measurements
- automated measurement and evaluation, making routine easy
- UV Add-on for curing of reactive polymers
Specification
- Temperature range: -170°C – 600°C
- Heating/Cooling rate: 0.001 K/min – 100 K/min
- Temperature accuracy: ± 0.1 K (indium)
- Enthalpy: accuracy < 1% for adamantan, indium, zinc; < 2% for most materials
- Cooling device options:
- Compressed air cooling (RT to 600°C)
- IC40 (-40°C to 600°C)
- IC70 (-70°C to 600°C)
- LN2 cooling, automatically controlled (-170°C to 600°C)
- Gas atmospheres: nert, oxidizing, static and dynamic operation
Why Choose Differential Scanning Calorimeter
Choose the Differential Scanning Calorimeter Caliris® Classic for its cutting-edge design, high precision, and user-friendly operation. This instrument features a compact footprint, freeing up valuable lab space while maintaining robust performance. Its LED touch display provides real-time updates, and the smart software ensures fast setup and automatic evaluation for routine testing. With advanced cooling options ranging from -170°C to 600°C, the system supports diverse applications under inert or oxidizing atmospheres. The integrated LabV® data management platform organizes and tracks measurements for efficient workflows. Designed to deliver accuracy within ±0.1 K and enthalpy errors below 1%, the DSC 300 Caliris® Classic guarantees dependable, repeatable results for all your thermal analysis needs.

Reviews
There are no reviews yet.